Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 1.10 J | 0.808 ft-lb | ExxonMobil Method |
ExxonMobil LLDPE LL 1002.09 Linear Low Density Polyethylene Resin Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat.. |
|||
Puncture Energy | 1.10 J | 0.808 ft-lb | ExxonMobil Method |
ExxonMobil LLDPE LL 1002.80 Linear Low Density Polyethylene Resin Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat.. |
|||
Puncture Energy | 1.10 J | 0.808 ft-lb | ExxonMobil Method |
ExxonMobil LLDPE LL 1002X75 Linear Low Density Polyethylene Resin Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat.. |