Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Puncture Energy = 1.48 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 2.00 - 32.0 J

@Temperature -30.0 - -30.0 °C
1.48 - 23.6 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 15.5 J Grade Count:6
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim..
Puncture Energy 2.00 - 32.0 J

@Temperature -30.0 - -30.0 °C
1.48 - 23.6 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 17.6 J Grade Count:5
Overview of materials for Polybutylene Terephthalate (PBT), Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Extrusion Grade". Each property range of values reported is minimum an..
Puncture Energy 2.00 - 2.00 J

@Temperature -30.0 - -30.0 °C
1.48 - 1.48 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 2.00 J Grade Count:1
Overview of materials for Nylon 66, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr..
Puncture Energy 2.00 J

@Temperature -30.0 °C
1.48 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Lanxess Durethan® AKV 30 GIT H2.0 900116 Nylon 66, 30% Glass Fiber
PA 66, injection molding grade, 30% glass fibers, suitable for GIT (gas assisted technology), good surface finish, good heat-ageing resistance
Puncture Energy 2.00 J

@Temperature -30.0 °C
1.48 ft-lb

@Temperature -22.0 °F
Conditioned; ISO 6603-2
Lanxess Durethan® AKV 30 GIT H2.0 900116 Nylon 66, 30% Glass Fiber
PA 66, injection molding grade, 30% glass fibers, suitable for GIT (gas assisted technology), good surface finish, good heat-ageing resistance
Puncture Energy 2.00 J
1.48 ft-lb
ISO 6603-2
Lanxess Durethan® BG 30 X 000000 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers/glass spheres, good surface, low warpage
Puncture Energy 2.00 J

@Temperature -30.0 °C
1.48 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Lanxess Durethan® BG 30 X H2.0 901510 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers/glass spheres, good surface, good heat-ageing resistance
Puncture Energy 2.00 J

@Temperature -30.0 °C
1.48 ft-lb

@Temperature -22.0 °F
Conditioned; ISO 6603-2
Lanxess Durethan® BG 30 X H2.0 901510 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers/glass spheres, good surface, good heat-ageing resistance
Puncture Energy 2.00 J
1.48 ft-lb
ISO 6603-2
Lanxess Durethan® BKV 15 G H2.0 900051 Copolyamide, 15% Glass Fiber
CoPA, injection molding grade, 15% glass fibers, better surface resistance to alcoholic calcium chloride-solution than BKV 15 H2.0, good heat-ageing resistance
Puncture Energy 2.00 J

@Temperature -30.0 °C
1.48 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Lanxess Pocan® DP 1105 000000 PBT
PBT, non-reinforced, injection molding, extrusion, improved flowability
Puncture Energy 2.00 J
1.48 ft-lb
53 N; 40µm sample; ASTM D5748
Borealis FA5223 Low Density Polyethylene
FA5223 is a Low Density Polyethylene for Film Extrusion. Contains antioxidant and antiblock additive. This grade is developed to give strong film for medium duty applications. Applications FA5223..
Puncture Energy 2.00 J
1.48 ft-lb
53 N; 40µm sample; ASTM D5748
Borealis FA5224 Low Density Polyethylene
FA5224 is a Low Density Polyethylene for Film Extrusion. Contains Antioxidant, Anti-block and Medium Slip additives. This grade is developed to give strong film for medium duty applications. Appl..
Copyright © lookpolymers.com All Rights Reserved