Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 1.50 - 1.50 J @Temperature -30.0 - -30.0 °C |
1.11 - 1.11 ft-lb @Temperature -22.0 - -22.0 °F |
Average value: 1.50 J Grade Count:1 |
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% .. |