Polymer Property : Puncture Energy = 11.8 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 16.0 J

@Temperature -30.0 °C
11.8 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Lanxess Pocan® B 1700 000000 PBT
PBT, non-reinforced, extrusion, food contact
Puncture Energy 16.0 J

@Temperature -40.0 °C
11.8 ft-lb

@Temperature -40.0 °F
Puncture Resistance at Max Load; ASTM D3763
Eastman Eastar MN004 Copolyester
Eastar Copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. Eastar MN004 contains a mold release.Appl..