Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 16.0 J @Temperature -30.0 °C |
11.8 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Lanxess Pocan® B 1700 000000 PBT PBT, non-reinforced, extrusion, food contact |
|||
Puncture Energy | 16.0 J @Temperature -40.0 °C |
11.8 ft-lb @Temperature -40.0 °F |
Puncture Resistance at Max Load; ASTM D3763 |
Eastman Eastar MN004 Copolyester Eastar Copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. Eastar MN004 contains a mold release.Appl.. |