Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 27.0 J | 19.9 ft-lb | Conditioned; ISO 6603-2 |
Lanxess Durethan® A 30 S 000000 Nylon 66 PA 66 standard injection molding-grade, non-reinforced, good demolding, very rapid solidificationApplication Examples: plug connectors, terminal blocks, cable clips, bobbins |