Puncture Energy 27.0 J
19.9 ft-lb
Conditioned; ISO 6603-2
Lanxess Durethan® A 30 S 000000 Nylon 66
PA 66 standard injection molding-grade, non-reinforced, good demolding, very rapid solidificationApplication Examples: plug connectors, terminal blocks, cable clips, bobbins