Polymer Property : Puncture Energy = 2.66 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 3.60 J
2.66 ft-lb
Conditioned; ISO 6603-2
Lanxess Durethan® AKV 30 G H2.0 SR1 900051 Nylon 66, 30% Glass Fiber
PA 66, injection molding grade, 30% glass fibers, better surface than AKV 30 H2.0, good heat-ageing resistance
Puncture Energy 3.60 J
2.66 ft-lb
ISO 6603-2
Lanxess Durethan® AKV 50 H2.0 901510 Nylon 66, 50% Glass Fiber
PA 66, injection molding grade, 50% glass fibers, good heat-ageing resistance