Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 39.0 J @Temperature -40.0 °C |
28.8 ft-lb @Temperature -40.0 °F |
Puncture Resistance at Max Load; ASTM D3763 |
Eastman Eastar EB062 Copolyester Eastar Copolyester EB062 is a resin specifically developed for extrusion blown bottles where aesthetics such as high clarity and gloss, coupled with design flexibility, drive demand. Compared to com.. |
|||
Puncture Energy | 39.0 J @Temperature -40.0 °C |
28.8 ft-lb @Temperature -40.0 °F |
Puncture Resistance at Max Load; ASTM D3763 |
Eastman Eastar MB002 Copolyester Eastar copolyester MB002 is a resin specifically developed for extrusion blow molding containers in medical applications where aesthetics such as high clarity and gloss, coupled with high toughness .. |
|||
Puncture Energy | 39.0 J @Temperature -40.0 °C |
28.8 ft-lb @Temperature -40.0 °F |
Puncture Resistance at Max Load; ASTM D3763 |
Eastman Provista MP002 Copolymer Provista Copolymer MP002 is a resin specifically developed for extrusion into profiles for medical applications where aesthetics such as high clarity and gloss, coupled with design flexibility and e.. |
|||
Puncture Energy | 39.0 J @Temperature -40.0 °C |
28.8 ft-lb @Temperature -40.0 °F |
Puncture Resistance at Max Load; ASTM D3763 |
Eastman Provista ST Copolymer Provista Copolymer ST is a resin specifically developed for profile extrusion where high clarity and gloss, toughness, and processability are critical. Provista Copolymer ST is a second-generation m.. |
|||
Puncture Energy | 39.0 J | 28.8 ft-lb | Puncture Resistance @Max Load, -10°C; ASTM D3763 |
Eastman TiGlaze SV Copolyester TiGLAZE SV copolyester is a specialty copolyester for the architectural glazing industry, designed to provide a unique balance of toughness, stiffness and material value. The material has a CC1 Ligh.. |
|||
Puncture Energy | 39.0 J @Temperature -40.0 °C |
28.8 ft-lb @Temperature -40.0 °F |
Puncture Resistance at Max Load; ASTM D3763 |
Eastman Eastar GN078 Copolyester, Natural Eastar Copolyester GN078 builds on the strength of Eastar Copolyester GN077 by offering improved melt strength and toughness. Eastar Copolyester GN078 does not meet FDA compliance but is an excellen.. |