Eastman Eastar GN078 Copolyester, Natural

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Unreinforced
Manufacturer Eastman Chemical
Trade Name Eastar
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman Eastar GN078 Copolyester, Natural.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Eastar Copolyester GN078 builds on the strength of Eastar Copolyester GN077 by offering improved melt strength and toughness. Eastar Copolyester GN078 does not meet FDA compliance but is an excellent product for large tough bottles not requiring this approval. Eastar Copolyester GN078 is an environmentally responsible material that contains no halogens or orthophthlate plasticizers.Applications/UsesNon-FDA EBM applications
Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D792
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Tensile Strength at Break 48.0 MPa
6960 psi
ASTM D638
Tensile Strength, Yield 47.0 MPa
6820 psi
ASTM D638
Elongation at Break 300 %
300 %
ASTM D638
Elongation at Yield 5.0 %
5.0 %
ASTM D638
Tensile Modulus 1.90 GPa
276 ksi
ASTM D638
Flexural Strength 65.0 MPa
9430 psi
ASTM D790
Flexural Modulus 1.90 GPa
276 ksi
ASTM D790
Izod Impact, Notched 0.630 J/cm

@Temperature -40.0 °C
1.18 ft-lb/in

@Temperature -40.0 °F
ASTM D256
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched NB
NB
ASTM D4812
NB

@Temperature -40.0 °C
NB

@Temperature -40.0 °F
ASTM D4812
Puncture Energy 41.0 J
30.2 ft-lb
Puncture Resistance @Max Load, 0°C; ASTM D3763
41.0 J
30.2 ft-lb
Puncture Resistance @Max Load, 23°C; ASTM D3763
39.0 J

@Temperature -40.0 °C
28.8 ft-lb

@Temperature -40.0 °F
Puncture Resistance at Max Load; ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 73.0 °C
163 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 63.0 °C
145 °F
ASTM D648
Vicat Softening Point 85.0 °C
185 °F
1kg load; ASTM D1525
Optical Properties Metric English Comments
Haze 1.3 %
1.3 %
ASTM D1003
Gloss 143 %
143 %
at 60°; ASTM D2457
Transmission, Visible 87 %
87 %
Regular Transmittance; ASTM D1003
91 %
91 %
Total Transmittance; ASTM D1003
Descriptive Properties Value Comments
Color, CIE a* -0.2
ASTM D2244
Color, CIE b* 0.6
ASTM D2244
Color, CIE L* 95
ASTM D2244