Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 5.00 J | 3.69 ft-lb | Conditioned; ISO 6603-2 |
Lanxess Durethan® AKV 50 H2.0 901510 Nylon 66, 50% Glass Fiber PA 66, injection molding grade, 50% glass fibers, good heat-ageing resistance |
|||
Puncture Energy | 5.00 J | 3.69 ft-lb | ISO 6603-2 |
Lanxess Durethan® DP 2131/20 H2.0 900051 Nylon 6, 20% Glass Fiber PA 6, injection molding grade, 20% glass fibers, better surface resistance to alcoholic calcium chloride-solution than BKV 20 H2.0, good heat-ageing resistance and weather resistance |
|||
Puncture Energy | 5.00 J @Temperature -30.0 °C |
3.69 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Lanxess Pocan® B 1305 000000 PBT PBT, non-reinforced, injection molding |
|||
Puncture Energy | 5.00 J | 3.69 ft-lb | ISO 6603-2 |
Lanxess Durethan® DP 2131/20 W1 901317 Nylon 6, 20% Glass Fiber PA 6, injection molding grade, 20% glass fibers, better surface finish and resistance to alcoholic calcium chloride-solution than BKV 20 H2.0, weather resistance, good heat-ageing resistance |
|||
Puncture Energy | 5.00 J | 3.69 ft-lb | ASTM 5748 |
Borealis Borstar® FB2230 LLDPE for Film Borstar BF2230 is a high molecular weight low density polyethylene film grade combining good and flexible extrusion behavior, excellent draw down and superior mechanical properties. Film made from .. |
|||
Puncture Energy | 5.00 J | 3.69 ft-lb | 130 N; 125µm sample; ASTM D5748 |
Borealis FA3220 Low Density Polyethylene FA3220 is a Low Density Polyethylene for Film Extrusion. Autoclave Technology. Unmodified. This grade is developed to give a strong film with balanced shrink properties. Applications FA3220 has bee.. |
|||
Puncture Energy | 5.00 J | 3.69 ft-lb | 130 N; 125µm sample; ASTM D5748 |
Borealis FA3227 Low Density Polyethylene FA3227 is a Low Density Polyethylene for Film Extrusion. Autoclave Technology. Heat and U/V stabilized. This grade is suitable for building construction film and meets the requirements for heat, al.. |
|||
Puncture Energy | 5.00 J | 3.69 ft-lb | ASTM 5748 |
Borealis Borstar® FB2310 LLDPE for Film Borstar BF2310 is a high molecular weight low density polyethylene film grade combining good and flexible extrusion behavior, excellent draw down and superior mechanical properties. Film made from .. |