Puncture Energy 36.0 J
26.6 ft-lb
Puncture Resistance @Max Load, 23°C; ASTM D3763
Eastman Eastar GN046 Copolyester, Natural
Eastar Copolyester GN046 is a very high melt strength copolyester targeted for extrusion blow molding applications. Blow molding of large parts (up to several pounds) are possible with this material..