Mechanical Properties Metric English Comments
Puncture Energy 49.0 J

@Temperature -40.0 °C
36.1 ft-lb

@Temperature -40.0 °F
Puncture Resistance at Max Load; ASTM D3763
Eastman Eastalloy DA510 Polymer  (discontinued **)
Eastalloy Polymer DA510 is a clear copolyester/polycarbonate alloy. This product has good physical properties. These include good impact strength, chemical resistance, heat resistance, dimensional s..
Puncture Energy 49.0 J

@Temperature -40.0 °C
36.1 ft-lb

@Temperature -40.0 °F
Puncture Resistance at Max Load; ASTM D3763
Eastman Eastalloy MA510 Polymer  (discontinued **)
Eastalloy MA510 Polymer is a clear copolyester/polycarbonate alloy. It affords the consumer excellent impact strength, chemical resistance, dimensional stability, low shrinkage rates and other enhan..
Puncture Energy 49.0 - 49.0 J

@Temperature -40.0 - -40.0 °C
36.1 - 36.1 ft-lb

@Temperature -40.0 - -40.0 °F
Average value: 49.0 J Grade Count:2
Overview of materials for Polycarbonate/PET Polyester Blend
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values..