Mechanical Properties Metric English Comments
Puncture Energy 4.52 J
3.33 ft-lb
ExxonMobil Method
ExxonMobil Exceed™ 1015HA Metallocene Polyethylene Resin
Product Description: Exceed 1015 mVLDPE resin is metallocene ethylene-hexene copolymer. Films made from Exceed 1015 mVLDPE have outstanding cold temperature toughness, impact strength and puncture. ..