Mechanical Properties Metric English Comments
Puncture Energy 50.0 - 65.0 J
36.9 - 47.9 ft-lb
Average value: 58.9 J Grade Count:14
Overview of materials for Polycarbonate, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp..
Puncture Energy 50.0 - 55.0 J
36.9 - 40.6 ft-lb
Average value: 51.5 J Grade Count:10
Overview of materials for Polycarbonate, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of..
Puncture Energy 50.0 - 65.0 J

@Temperature -30.0 - -30.0 °C
36.9 - 47.9 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 61.3 J Grade Count:4
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max..
Puncture Energy 50.0 - 60.0 J
36.9 - 44.3 ft-lb
Average value: 58.1 J Grade Count:16
Overview of materials for Polycarbonate, UV Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a..
Puncture Energy 50.0 J
36.9 ft-lb
ISO 6603-2
Lanxess Durethan® DP 2325 H3.0 000000 Nylon 66
PA 66, injection molding grade, non-reinforced, elastomer-modified, good heat-ageing resistance, extremely high notched impact strength even at dry state and at low temperatures
Puncture Energy 50.0 J
36.9 ft-lb
ISO 6603-2
Covestro Apec® DP1-9389/5 Polycarbonate
Developmental producteasy flowingeasy to demoldsoftening temperature (VST/B 120)=218 °CPreprocessingMax. Water content
Puncture Energy 50.0 J
36.9 ft-lb
ISO 6603-2
Covestro Makrolon® 1837* Polycarbonate, Impact Grade
ISO 7391-PC,MP,(,,)-09-9Global gradeFormerly Makrolon DP1-1837MVR (300 °C/1.2 kg) 11 cm3/10 minImpact modifiedMedium viscosityEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable..
Puncture Energy 50.0 J
36.9 ft-lb
ISO 6603-2
Covestro Makrolon® 1899* Polycarbonate, Impact Grade
Formerly Makrolon DP1-1899MVR (300 °C/1.2 kg) 15.5 cm³/10 minspecial flame retardant systemUL 94V-0/0.75 mmImpact modifiedMedium viscosityEasy releaseVicat softening temperature 50 N; 50 °C/h = 1..
Puncture Energy 50.0 J
36.9 ft-lb
ISO 6603-2
Covestro Makrolon® 6265 Polycarbonate, Flame Retardant Grade
ISO 7391-PC,MFR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 19 cm3/10 minFlame retardantUL 94V-0/1.5 mmLow viscosityEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in opaque co..
Puncture Energy 50.0 J
36.9 ft-lb
ISO 6603-2
Covestro Makrolon® 6267 Polycarbonate, Flame Retardant Grade
ISO 7391-PC,MFLR,(,,)-18-9Formerly Makrolon DP1-1872MVR (300 °C/1.2 kg) 19 cm3/10 minFlame retardantUL 94V-0/1.5 mmLow viscosityUV stabilizedEasy releaseInjection molding - Melt temperature 280 - 3..
Puncture Energy 50.0 J
36.9 ft-lb
ISO 6603-2
Covestro Makrolon® 6585 Polycarbonate, Flame Retardant Grade
ISO 7391-PC,MFR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minFlame retardantUL 94V-0/1.2 mm5VA/3.0 mm and 5VB (WT) /2.0 mmHigh viscosityEasy releaseInjection molding - Melt temperature 28..
Puncture Energy 50.0 J
36.9 ft-lb
ISO 6603-2
Covestro Makrolon® LED2045 Polycarbonate
ISO 7391-PC,MRT,(,,)-24-9Global gradeMVR (250 °C/2.16 kg) 16.5 cm3/10minLight guidesPC with highest transmissionLow viscosityEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable ..
Puncture Energy 50.0 J
36.9 ft-lb
ISO 6603-2
Covestro Makrolon® 1260 Polycarbonate, Impact Grade
ISO 7391-PC,MPR,(,,)-24-9Global gradeMVR (300 °C/1.2 kg) 34 cm3/10 minImpact modifiedLow viscosityEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in light colors onlyPreproc..
Puncture Energy 50.0 J
36.9 ft-lb
ISO 6603-2
Covestro Makrolon® 6487 Polycarbonate, Flame Retardant Grade
ISO 7391-PC,MFLR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12.5 cm3/10 minFlame retardantUL 94V-0/1.5 mm and 5VA/3.0 mmMedium viscosityUV stabilizedEasy releaseInjection molding - Melt temperature 2..
Puncture Energy 50.0 J
36.9 ft-lb
ISO 6603-2
Covestro Makrolon® OD2015 Polycarbonate
Global gradeOptical storage mediaLow viscosityEasy releaseHigh purityInjection moldingAvailable in natural color onlyPreprocessingMax. Water content
Puncture Energy 50.0 - 65.0 J
36.9 - 47.9 ft-lb
Average value: 60.8 J Grade Count:4
Overview of materials for Nylon 6, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri..
Puncture Energy 50.0 - 67.0 J

@Temperature -30.0 - -30.0 °C
36.9 - 49.4 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 60.9 J Grade Count:3
Overview of materials for Nylon 6, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri..
Puncture Energy 50.0 - 67.0 J

@Load <=5810 kg
36.9 - 49.4 ft-lb

@Load <=12800 lb
Average value: 60.9 J Grade Count:3
Overview of materials for Nylon 6, Impact Grade