Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 8.25 J | 6.08 ft-lb | Dow Method |
Dow ELITE™ 5500G Enhanced Polyethylene Resin ™ 5500G is a copolymer produced via INSITE™ Technology. It offers an exceptional combination of processability, low heat seal initiation temperature, package integrity, optical properties, and te.. |
|||
Puncture Energy | 8.25 J | 6.08 ft-lb | Dow Method |