Polymer Property : Puncture Energy = 8.85 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 12.0 J
8.85 ft-lb
Puncture Resistance @ max load, 23°C; ISO 6603-2
Eastman Eastar GN002 Copolyester, Natural  (discontinued **)
Eastar GN002 Copolyester is a glycol modified polyethylene terephthalate (PET) with an added mold release. Eastar GN002 copolyester will not crystallize and thus offers wider processing latitude tha..
Puncture Energy 12.0 J
8.85 ft-lb
Puncture Resistance @ max load, 23°C; ISO 6603-2
Eastman Eastar GN005 Copolyester, Natural  (discontinued **)
Eastar GN005 Copolyester is a glycol modified polyethylene terephthalate (PET) with an added mold release. Eastar GN005 copolyester will not crystallize and thus offers wider processing latitude tha..
Puncture Energy 12.0 J
8.85 ft-lb
ISO 6603-2
Lanxess Durethan® B 30 S 000000 Nylon 6
PA 6, injection molding-grade, non-reinforced, easy-flow, easy-release, rapid solidification
Puncture Energy 12.0 J
8.85 ft-lb
Conditioned; ISO 6603-2
Lanxess Durethan® BKV 30 HTS 901510 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers, very good heat-ageing resistance
Puncture Energy 12.0 J
8.85 ft-lb
Puncture Resistance @ max load, 23°C; ISO 6603-2
Eastman Drystar 0113 Copolyester
This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen..
Puncture Energy 12.0 - 41.0 J
8.85 - 30.2 ft-lb
Average value: 25.7 J Grade Count:8
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m..