Polymer Property : Torsional Stiffness = 22.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Torsional Stiffness 22.0 MPa
3190 psi
+20°C; ASTM D1043
C.O.I.M. LARIPUR® LPR5260 PTMG Polyether Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..
Torsional Stiffness 22.0 - 472 MPa
3190 - 68500 psi
Average value: 181 MPa Grade Count:5
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyether Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyether Grade". Each property range of values reported is minimum a..