Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Torsional Stiffness | 22.0 - 472 MPa | 3190 - 68500 psi | Average value: 181 MPa Grade Count:5 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyether Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyether Grade". Each property range of values reported is minimum a.. |