Polymer Property : Modulus of Rupture = 0.03924 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Rupture 0.03924 GPa

@Temperature 1500 °C,
Time 10800 sec
5.691 ksi

@Temperature 2730 °F,
Time 3.00 hour
Chosun Refractories HSC-18SC Dense and High-Strength Castable, Superdense
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.03924 GPa

@Temperature 250 °C
5.691 ksi

@Temperature 482 °F
Chosun Refractories SBSN-G15 Nozzle
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.03924 - 0.07848 GPa

@Temperature 1300 °C,
Time 10800 sec
5.691 - 11.38 ksi

@Temperature 2370 °F,
Time 3.00 hour
Chosun Refractories PTC-130S Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).