Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.0007848 - 0.0017658 GPa @Temperature 1000 °C, Time 10800 sec |
0.1138 - 0.25611 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories GUN-120L Light-Weight Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |