Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.000900 GPa @Temperature 104 °C |
0.131 ksi @Temperature 219 °F |
Dried; ASTM C268 |
BNZ Materials Bazelite 2300 Insulating Castable Blaz 2300 is a lightweight, general purpose insulating castable. Can be used for back-up or exposed to furnace conditions. Used for one-shot linings, petrochemical heaters, combustion chambers and f.. |
|||
Modulus of Rupture | 0.000900 GPa @Temperature 104 °C |
0.131 ksi @Temperature 219 °F |
Dried; ASTM C268 |
BNZ Materials Bazelite 2300 LI Insulating Castable Blaz 2300 L is similar to Blaz 2300 but suitable for those applications where reducing conditions might be encountered. These high purity, low iron products are specifically designed for both back-u.. |
|||
Modulus of Rupture | 0.000900 GPa @Temperature 1095 °C |
0.131 ksi @Temperature 2003 °F |
ASTM C268 |
BNZ Materials Bazelite 2100 Insulating Castable Blaz 2100 is a general purpose lightweight castable for use as an exposed hot face refractory or as a very thermally efficient back-up to a dense refractory lining. Can be installed by casting, gunn.. |