Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.000981 - 0.001962 GPa @Temperature 1000 °C, Time 10800 sec |
0.142 - 0.2846 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories GUN-140L Light-Weight Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.000981 - 0.001962 GPa @Temperature 500 °C, Time 10800 sec |
0.142 - 0.2846 ksi @Temperature 932 °F, Time 3.00 hour |
|
Chosun Refractories INCT-100N Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.000981 GPa @Temperature 1500 °C, Time 10800 sec |
0.142 ksi @Temperature 2730 °F, Time 3.00 hour |
|
Chosun Refractories M55 Special High-Density Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.000981 - 0.0024525 GPa @Temperature 1000 °C, Time 10800 sec |
0.142 - 0.35571 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories MIX-1(1:4) Light-Weight Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.000981 - 0.001962 GPa @Temperature 1000 °C, Time 10800 sec |
0.142 - 0.2846 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories GUN-135L Light-Weight Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.000981 - 0.003924 GPa @Temperature 1350 °C, Time 10800 sec |
0.142 - 0.5691 ksi @Temperature 2460 °F, Time 3.00 hour |
|
Chosun Refractories PAC-160 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.000981 - 0.003924 GPa @Temperature 1500 °C, Time 10800 sec |
0.142 - 0.5691 ksi @Temperature 2730 °F, Time 3.00 hour |
|
Chosun Refractories PAC-160 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |