Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Mechanical Properties Metric English Comments
Modulus of Rupture 2.41e-7 - 0.00147 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000349 - 0.213 ksi

@Temperature 230 °F,
Time 24.0 hour
0.000981 - 0.001962 GPa

@Temperature 500 °C,
Time 10800 sec
0.142 - 0.2846 ksi

@Temperature 932 °F,
Time 3.00 hour
Compressive Strength 3.92 - 6.86 MPa

@Temperature 500 °C,
Time 10800 sec
569 - 996 psi

@Temperature 932 °F,
Time 3.00 hour
Cold Crushing Strength
4.90 - 7.85 MPa

@Temperature 110 °C,
Time 86400 sec
711 - 1140 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.291 W/m-K

@Temperature 260 °C
2.01 BTU-in/hr-ft²-°F

@Temperature 500 °F
0.3257 W/m-K

@Temperature 540 °C
2.257 BTU-in/hr-ft²-°F

@Temperature 1000 °F
0.3606 W/m-K

@Temperature 800 °C
2.498 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Maximum Service Temperature, Air 1000 °C
1830 °F
limited
Shrinkage -0.600 %

@Temperature 1350 °C,
Time 10800 sec
-0.600 %

@Temperature 2460 °F,
Time 3.00 hour
-0.0600 %

@Temperature 110 °C,
Time 86400 sec
-0.0600 %

@Temperature 230 °F,
Time 24.0 hour
Component Elements Properties Metric English Comments
Al2O3 25 %
25 %
SiO2 50 %
50 %
Descriptive Properties Value Comments
Installation Method Casting, Troweling
Main Applications Low temperature Various furnaces
Material Required for Estimating (kg/?) 1,250