Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00103 GPa @Temperature 104 °C |
0.149 ksi @Temperature 219 °F |
Dried; ASTM C258 |
BNZ Materials Bazelite 2000 Insulating Castable BNZ manufactures a variety of insulating and dense castable refractories to meet the exacting needs of the high temperature processing industries. These hydraulic setting products are suitable for i.. |
|||
Modulus of Rupture | 0.00103 GPa @Temperature 540 °C |
0.149 ksi @Temperature 1000 °F |
Fired; ASTM C268 |
BNZ Materials Bazelite 2300 LI Insulating Castable Blaz 2300 L is similar to Blaz 2300 but suitable for those applications where reducing conditions might be encountered. These high purity, low iron products are specifically designed for both back-u.. |
|||
Modulus of Rupture | 0.00103 GPa @Temperature 815 °C |
0.149 ksi @Temperature 1500 °F |
ASTM C268 |
BNZ Materials Bazelite 2100 Insulating Castable Blaz 2100 is a general purpose lightweight castable for use as an exposed hot face refractory or as a very thermally efficient back-up to a dense refractory lining. Can be installed by casting, gunn.. |