Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Rupture = 0.213 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Rupture 2.41e-7 - 0.00147 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000349 - 0.213 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories GUN-80L Light-Weight Gunning Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 2.41e-7 - 0.00147 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000349 - 0.213 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories INCT-100N Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 3.37e-7 - 0.00147 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000489 - 0.213 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories INCT-110N Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 3.37e-7 - 0.00147 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000489 - 0.213 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories INCT-120N Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 3.37e-7 - 0.00147 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000489 - 0.213 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories INCT-135N Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 3.37e-7 - 0.00147 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000489 - 0.213 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories INCT135S Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 4.33e-7 - 0.00147 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000628 - 0.213 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories INCT-140 Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 4.33e-7 - 0.00147 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000628 - 0.213 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories INCT-160 Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).