Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Rupture 5.77e-7 - 0.00294 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000837 - 0.427 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories INCT-170 Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 5.77e-7 - 0.00294 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000837 - 0.427 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories PTF-180 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 5.77e-7 - 0.00294 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000837 - 0.427 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories TPA-175 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).