Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 5.77e-7 - 0.00294 GPa @Temperature 110 °C, Time 86400 sec |
0.0000837 - 0.427 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories INCT-170 Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 5.77e-7 - 0.00294 GPa @Temperature 110 °C, Time 86400 sec |
0.0000837 - 0.427 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories PTF-180 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 5.77e-7 - 0.00294 GPa @Temperature 110 °C, Time 86400 sec |
0.0000837 - 0.427 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories TPA-175 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |