Mechanical Properties Metric English Comments
Modulus of Rupture 0.004905 GPa

@Temperature 110 °C,
Time 86400 sec
0.7114 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories APC-120 Acid-proof Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.004905 GPa

@Temperature 1400 °C
0.7114 ksi

@Temperature 2550 °F
Chosun Refractories CRMG-S02 Long Stopper
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.004905 - 0.008829 GPa

@Temperature 1500 °C,
Time 10800 sec
0.7114 - 1.281 ksi

@Temperature 2730 °F,
Time 3.00 hour
Chosun Refractories HACT-170 High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.004905 GPa

@Temperature 110 °C,
Time 86400 sec
0.7114 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories HSC-15G Dense and High-Strength Castable, Credens
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.004905 GPa

@Temperature 110 °C,
Time 86400 sec
0.7114 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories M55 Special High-Density Gunning Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.004905 - 0.007848 GPa

@Temperature 1500 °C,
Time 10800 sec
0.7114 - 1.138 ksi

@Temperature 2730 °F,
Time 3.00 hour
Chosun Refractories PT-160 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.004905 - 0.007848 GPa

@Temperature 1500 °C,
Time 10800 sec
0.7114 - 1.138 ksi

@Temperature 2730 °F,
Time 3.00 hour
Chosun Refractories PT-165 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.004905 GPa

@Temperature 1500 °C,
Time 10800 sec
0.7114 ksi

@Temperature 2730 °F,
Time 3.00 hour
Chosun Refractories SW83 Special High-Density Gunning Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.004905 GPa

@Temperature 110 °C,
Time 86400 sec
0.7114 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories TCH-175SV Torpedo Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.004905 - 0.008829 GPa

@Temperature 1500 °C,
Time 10800 sec
0.7114 - 1.281 ksi

@Temperature 2730 °F,
Time 3.00 hour
Chosun Refractories HACT-165 High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).