Chosun Refractories APC-120 Acid-proof Castable

Category Ceramic , Oxide , Silicon Oxide
Manufacturer Chosun Refractories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories APC-120 Acid-proof Castable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Mechanical Properties Metric English Comments
Modulus of Rupture 0.004905 GPa

@Temperature 110 °C,
Time 86400 sec
0.7114 ksi

@Temperature 230 °F,
Time 24.0 hour
0.007848 GPa

@Temperature 500 °C,
Time 10800 sec
1.138 ksi

@Temperature 932 °F,
Time 3.00 hour
0.00981 GPa

@Temperature 1000 °C,
Time 10800 sec
1.42 ksi

@Temperature 1830 °F,
Time 3.00 hour
Compressive Strength 11.8 MPa

@Temperature 110 °C,
Time 86400 sec
1710 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
29.4 MPa

@Temperature 500 °C,
Time 10800 sec
4270 psi

@Temperature 932 °F,
Time 3.00 hour
Cold Crushing Strength
34.3 MPa

@Temperature 1000 °C,
Time 10800 sec
4980 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1200 °C
2190 °F
limited
Shrinkage -0.500 %

@Temperature 1000 °C,
Time 10800 sec
-0.500 %

@Temperature 1830 °F,
Time 3.00 hour
-0.250 %

@Temperature 500 °C,
Time 10800 sec
-0.250 %

@Temperature 932 °F,
Time 3.00 hour
-0.100 %

@Temperature 110 °C,
Time 86400 sec
-0.100 %

@Temperature 230 °F,
Time 24.0 hour
Component Elements Properties Metric English Comments
Al2O3 40 %
40 %
SiO2 55 %
55 %
Descriptive Properties Value Comments
Installation Method Casting, Vibrating
Main Applications Chemical Plant
Material Required for Estimating (kg/?) 2,000
Water Required for Casting(%) 15
Users viewing this material also viewed the following: