Mechanical Properties Metric English Comments
Modulus of Rupture 0.0200 GPa

@Temperature 110 °C
2.90 ksi

@Temperature 230 °F
Cold
Sharadaa Ceramics VELECRETE RC 101 Rodding Castables
Description: The Rodding Castables offered by us are user friendly in nature and does not require high energy mixing machines and vibrators. Free flowing in nature, these castables are designed in c..
Modulus of Rupture 0.0200 GPa

@Temperature 1400 °C
2.90 ksi

@Temperature 2550 °F
Cold
Sharadaa Ceramics VELECRETE RC 101 Rodding Castables
Description: The Rodding Castables offered by us are user friendly in nature and does not require high energy mixing machines and vibrators. Free flowing in nature, these castables are designed in c..
Modulus of Rupture 0.0200 GPa

@Temperature 1100 °C
2.90 ksi

@Temperature 2010 °F
Hot
Sharadaa Ceramics VELECRETE RC 104 Rodding Castables
Description: The Rodding Castables offered by us are user friendly in nature and does not require high energy mixing machines and vibrators. Free flowing in nature, these castables are designed in c..
Modulus of Rupture 0.0200 GPa

@Temperature 110 °C
2.90 ksi

@Temperature 230 °F
Cold
Sharadaa Ceramics VELECRETE RC 105 Rodding Castables
Description: The Rodding Castables offered by us are user friendly in nature and does not require high energy mixing machines and vibrators. Free flowing in nature, these castables are designed in c..
Modulus of Rupture 0.0200 GPa

@Temperature 1400 °C
2.90 ksi

@Temperature 2550 °F
Cold
Sharadaa Ceramics VELECRETE RC 105 Rodding Castables
Description: The Rodding Castables offered by us are user friendly in nature and does not require high energy mixing machines and vibrators. Free flowing in nature, these castables are designed in c..
Modulus of Rupture 0.0200 GPa

@Temperature 1100 °C
2.90 ksi

@Temperature 2010 °F
Hot
Sharadaa Ceramics VELECRETE RC 105 Rodding Castables
Description: The Rodding Castables offered by us are user friendly in nature and does not require high energy mixing machines and vibrators. Free flowing in nature, these castables are designed in c..
Modulus of Rupture 0.0200 GPa

@Temperature 1000 °C
2.90 ksi

@Temperature 1830 °F
Cold
Sharadaa Ceramics VELECRETE RC 108 Rodding Castables
Description: The Rodding Castables offered by us are user friendly in nature and does not require high energy mixing machines and vibrators. Free flowing in nature, these castables are designed in c..