Material Notes:
Description: The Rodding Castables offered by us are user friendly in nature and does not require high energy mixing machines and vibrators. Free flowing in nature, these castables are designed in compliance with international standards.Bond: UltrafineAggregate: Andalusite + Cal.BauxiteType of Setting: HydraulicInformation provided by Sharadaa Ceramics Pvt. Ltd.
Physical Properties Metric English Comments
Bulk Density 2.80 g/cc
0.101 lb/in³
After Drying at 110°C
Grain Size <= 10000 µm
<= 10000 µm
Mechanical Properties Metric English Comments
Modulus of Rupture 0.0200 GPa

@Temperature 1000 °C
2.90 ksi

@Temperature 1830 °F
Cold
0.0240 GPa

@Temperature 110 °C
3.48 ksi

@Temperature 230 °F
Cold
0.0240 GPa

@Temperature 1400 °C
3.48 ksi

@Temperature 2550 °F
Cold
0.0250 GPa

@Temperature 1100 °C
3.63 ksi

@Temperature 2010 °F
Hot
Compressive Strength 100 MPa

@Temperature 1000 °C
14500 psi

@Temperature 1830 °F
Cold Crushing
120 MPa

@Temperature 110 °C
17400 psi

@Temperature 230 °F
Cold Crushing
120 MPa

@Temperature 1400 °C
17400 psi

@Temperature 2550 °F
Cold Crushing
Thermal Properties Metric English Comments
Thermal Conductivity 2.09 W/m-K

@Temperature 600 °C
14.5 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Hot Face
Maximum Service Temperature, Air 1700 °C
3090 °F
Component Elements Properties Metric English Comments
Al2O3 68 %
68 %
Fe2O3 1.2 %
1.2 %
Descriptive Properties Value Comments
Permanent Linear Change 1
at 1700°C
Resistance to Accretion Excellent
Thermal Expansion 1
at 1100°C