Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tear Strength = 0.120 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 0.120 kN/m
0.685 pli
ASTM D 624
Eurofoam Evacell EVA 30 EVA + PE Foam
Foamed polyethylene charged with EVA, with extremely fine cells, excellent elasticity, resilience and mechanical resistance. It can be thermoformed several times. It has completely closed cells, di..
Tear Strength 0.120 kN/m
0.685 pli
ASTM D 624
Eurofoam Polycell PE 30 Polyethylene Foam
Closed-cell polyethylene foam. Extruded reticulated pieces. Excellent physical properties both for active and static uses. Adjustable softness, elasticity, thermal deformation, shock absorbing. Use..
Copyright © lookpolymers.com All Rights Reserved