Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 0.120 kN/m | 0.685 pli | ASTM D 624 |
Eurofoam Evacell EVA 30 EVA + PE Foam Foamed polyethylene charged with EVA, with extremely fine cells, excellent elasticity, resilience and mechanical resistance. It can be thermoformed several times. It has completely closed cells, di.. |
|||
Tear Strength | 0.120 kN/m | 0.685 pli | ASTM D 624 |
Eurofoam Polycell PE 30 Polyethylene Foam Closed-cell polyethylene foam. Extruded reticulated pieces. Excellent physical properties both for active and static uses. Adjustable softness, elasticity, thermal deformation, shock absorbing. Use.. |