Polymer Property : Tear Strength = 1.33 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 1.33 kN/m
7.62 pli
JIS K6301-B
Stellarchem DIOSHY® MP-960NC TPE Compound
This grade of Stellarchem MP series is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, styrene block copolymers based, ..