Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 1.33 kN/m | 7.62 pli | JIS K6301-B |
Stellarchem DIOSHY® MP-960NC TPE Compound This grade of Stellarchem MP series is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, styrene block copolymers based, .. |