Tear Strength 5.43 - 255 kN/m
31.0 - 1450 pli
Average value: 102 kN/m Grade Count:305
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyester Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyester Grade". Each property range of values reported is minimum a..