Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 5.43 kN/m | 31.0 pli | Trouser, PVC (80)/CP80AS2(20) |
Lubrizol Estane® CP80AS2 Thermoplastic Polyurethane Type: Estane® CP80AS2 is a soft, polyester based thermoplastic polyurethane resin.Features: Outstanding compatibility with flexible PVC allowing easy dispersion without pre-compounding.Uses: Tube/H.. |
|||
Tear Strength | 5.43 - 255 kN/m | 31.0 - 1450 pli | Average value: 102 kN/m Grade Count:305 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyester Grade". Each property range of values reported is minimum a.. |