Polymer Property : Tear Strength = 155 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength >= 27.2 kN/m
>= 155 pli
ASTM D624
Multibase Multi-Flex® TPE D 4210 BLK
The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Tear Strength 27.1 kN/m
155 pli
ASTM D624
Network Polymers Softflex® 0921
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.
Tear Strength 27.2 kN/m
155 pli
Total Finaprene® 602 Styrene-Butadiene TPE Copolymer Compound, Formulated to 57 Shore A  (discontinued **)
Styrene-Butadiene CopolymerDescription: Finaprene® 602 is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its broad molecular weight distribution, Finaprene® 60..
Tear Strength 27.1 kN/m
155 pli
Total Finaprene® 602 Styrene-Butadiene TPE Copolymer Compound, Formulated to 58 Shore A  (discontinued **)
Styrene-Butadiene CopolymerDescription: Finaprene® 602 is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its broad molecular weight distribution, Finaprene® 60..
Tear Strength 27.2 kN/m
155 pli
Injection molded plaques, Die C, Machine Direction; ASTM D624
Kraton® G2705 GU (SEBS) Compound
Description: Kraton G2705 GU-N is an easy processing material designed for applications where FDA regulations are required. The material exhibits high resilience, low compression set, and good punct..
Tear Strength 27.2 kN/m
155 pli
Die B, post cured- 4 hours at 177°C; ASTM D624
Multibase C6-515 Dow-Corning Class VI Elastomer
Information provided by Multibase
Tear Strength 27.2 kN/m
155 pli
Initial Tear Strength
Saint-Gobain CHR® 6004 Glass-Foil Backing Silicone Adhesive Pressure Sensitive Tape
Description: For applications requiring higher tear strengths, fiberglass laminated with aluminum is available. Service temperatures range from -100°F to 500°F (-73°C to +260°C). This ta..
Tear Strength 27.2 kN/m
155 pli
Die C (graves), 20 in/min; ASTM D624
PolyOne Synprene® IT 37-023 Thermoplastic Elastomer - SBC, Mineral Filled  (discontinued **)
Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledApplications:General PurposeMarket:Consumer GoodsIndustrialProcessing Method:Injection MoldingPolyOne First ChoiceInformation ..