Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 27.1 kN/m | 155 pli | ASTM D624 |
Network Polymers Softflex® 0921 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Tear Strength | 27.1 kN/m | 155 pli | |
Total Finaprene® 602 Styrene-Butadiene TPE Copolymer Compound, Formulated to 58 Shore A
(discontinued **) Styrene-Butadiene CopolymerDescription: Finaprene® 602 is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its broad molecular weight distribution, Finaprene® 60.. |