Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 32.1 kN/m | 183 pli | post cured- 2 hours at 177°C; Die B |
Multibase SILASTIC® C7-4565 TBPB Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tear Strength | 32.0 kN/m | 183 pli | D624 |
Polykemi AB POLYelast TPE Z706 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Tear Strength | 32.0 kN/m | 183 pli | D624 |
Polykemi AB POLYelast TPE Z706EX Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Tear Strength | 32.1 kN/m | 183 pli | 73°F, Die C; ASTM D624 |
ExxonMobil Vyram™ 9101-75 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi.. |
|||
Tear Strength | 32.0 kN/m | 183 pli | Die C |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 0.0 PHR Zinc Stearate MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tear Strength | 32.0 kN/m | 183 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ FSL 7661 Fluorinated Liquid Silicone Rubber This LSR elastomer is a fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperature.. |
|||
Tear Strength | 32.0 kN/m | 183 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LIM 6041 Liquid Silicone Rubber - Healthcare Radio Opaque (X-Ray Detectability) LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Tear Strength | 32.0 - 44.0 kN/m | 183 - 251 pli | NF EN ISO 1421 |
Isoflon Tisoflon® 14S Silicone Coated Glass Fabric Silicone coated Glass fabric TISOFLON®Information provided by Isoflon. |
|||
Tear Strength | 32.0 kN/m | 183 pli | |
Shin-Etsu Silicones LIMSâ„¢ KEG2000-40A/B Elastomer KEG2000-40 is a fast cure type liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is low enough to.. |
|||
Tear Strength | 32.1 kN/m | 183 pli | ASTM D624 |
STAR Thermoplastic Alloys & Rubbers StarMediflex P 7070-1000 TPE Product Description: StarMediflex P 7070-1000 is an easy processing TPE designed for injection molding. This particular class of TPE material for medical products and tubing applications. Features:S.. |
|||
Tear Strength | 32.0 kN/m | 183 pli | Die C; Cross direction; ASTM D624 |
Teknor Apex Sarlink® 3160 Thermoplastic Elastomer A low hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3160 can be processed by injection molding or extrusion for ap.. |
|||
Tear Strength | 32.0 kN/m | 183 pli | Die C; Cross direction; ASTM D624 |
Teknor Apex Sarlink® 3460 Thermoplastic Elastomer A NSF certified, low hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inject.. |
|||
Tear Strength | 32.0 kN/m | 183 pli | ASTM D2240 |
UBE UBEPOL BR130B Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE. |
|||
Tear Strength | 32.0 kN/m | 183 pli | |
Trelleborg R320 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Tear Strength | 32.0 kN/m | 183 pli | Die C |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 0.0 PHR Zinc Stearate MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tear Strength | 32.0 kN/m | 183 pli | ASTM D624 |
ELASTO UK Dryflex® 400701S SBS Based Material, 70A Hardness, Natural The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Tear Strength | 32.0 kN/m | 183 pli | ASTM D624 |
ELASTO UK Dryflex® 402701S SBS Based Material, 70A Hardness, Black The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Tear Strength | 32.0 kN/m | 183 pli | ASTM D624 |
ELASTO UK Dryflex® 500700S SEBS Based Material, Unfilled Qualities, 70A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Tear Strength | 32.0 kN/m | 183 pli | ASTM D624 |
ELASTO UK Dryflex® 502700S SEBS Based Material, Unfilled Qualities, 70A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Tear Strength | 32.0 kN/m | 183 pli | ASTM D624 |
ELASTO UK Dryflex® 600700S SEBS Based Material, Filled Qualities, 70A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Tear Strength | 32.0 kN/m | 183 pli | ASTM D624 |
ELASTO UK Dryflex® 602700S SEBS Based Material, Filled Qualities, 70A Hardness, Black The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Tear Strength | 32.1 kN/m | 183 pli | 73°C, Die C; ASTM D624 |
ExxonMobil Santoprene® 8201-60 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w.. |
|||
Tear Strength | 32.0 kN/m | 183 pli | ISO 34-B |
AlphaGary Evoprene™ 022 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
Tear Strength | 32.0 kN/m | 183 pli | Die C; Cross direction; ASTM D624 |
Teknor Apex Sarlink® 3460N Thermoplastic Elastomer A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext.. |
|||
Tear Strength | 32.1 kN/m | 183 pli | 73°F, Die C; ASTM D624 |
ExxonMobil Vyram™ 9201-75 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character.. |