ELASTO UK Dryflex® 400701S SBS Based Material, 70A Hardness, Natural

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer ELASTO UK Ltd, a Hexpol company
Trade Name Dryflex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ELASTO UK Dryflex® 400701S SBS Based Material, 70A Hardness, Natural.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for a fast and stable manufacturing process.Information from Vita Thermoplastic Polymers (VTP).Vita Thermoplastic Polymers was aquired by HEXPOL and is now ELASTO
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Linear Mold Shrinkage 0.0080 - 0.020 cm/cm
0.0080 - 0.020 in/in
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 70

@Thickness 4.00 mm
70

@Thickness 0.157 in
ASTM D2240
Tensile Strength at Break 4.00 MPa
580 psi
ASTM D638
Elongation at Break >= 500 %
>= 500 %
ASTM D638
100% Modulus 0.00300 GPa
0.435 ksi
ASTM D638
300% Modulus 0.00400 GPa
0.580 ksi
ASTM D638
Tear Strength 32.0 kN/m
183 pli
ASTM D624
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 75.0 °C
167 °F
Minimum Service Temperature, Air -50.0 °C
-58.0 °F
Processing Properties Metric English Comments
Processing Temperature 170 - 210 °C
338 - 410 °F
Descriptive Properties Value Comments
Bonding to PP Excellent
Chemical Resistance Good
Excluding organic solvents, aromatic and vegetable oils
Color Natural
Weather Resistance Moderate
Air ageing