Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 32.8 kN/m
187 pli
Die B, post cured- 8 hours at 200°C; ASTM D624
Multibase SILASTIC® 7-6830 Dow-Corning Biomedical Grade Liquid Silicone Rubber
Information provided by Multibase
Tear Strength 32.8 kN/m
187 pli
Notched, Die B; ASTM D 624
CPT C-Flex® R70-028 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Tear Strength 32.8 kN/m
187 pli
Die B; Silicone Property; Arlon SQA-TMS-029
Arlon T3020-B004 0.020" Self-Fusing, Cured Silicone Rubber Tape with Fiberglass Substrate
1.0 inch wide, 20 mil thick, black, rectangular cross-section, self-fusing silicone tape.Design/Construction:Side 1: Cured Silicone RubberSubstrate: 25% Sinusoidal FiberglassSide 2: Cured Silicone..
Tear Strength 32.8 kN/m
187 pli
Die B; Silicone Property; Arlon SQA-TMS-029
Arlon T3020-B002-## 0.020" Self-Fusing, Cured Silicone Rubber Tape with Fiberglass Substrate
0.5 inch wide, 20 mil thick, black, rectangular cross-section, self-fusing silicone tape. Product is supplied in various yard long roll lengths as indicated by the ## characters in the part number...