Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon T3020-B002-## 0.020" Self-Fusing, Cured Silicone Rubber Tape with Fiberglass Substrate

Category Polymer , Thermoset , Silicone , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon T3020-B002-## 0.020" Self-Fusing, Cured Silicone Rubber Tape with Fiberglass Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
0.5 inch wide, 20 mil thick, black, rectangular cross-section, self-fusing silicone tape. Product is supplied in various yard long roll lengths as indicated by the ## characters in the part number.Design/Construction:Side 1: Cured Silicone RubberSubstrate: 25% Sinusoidal FiberglassSide 2: Cured Silicone RubberInterleave: 1 mil PETThis data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 203 microns
8.00 mil
Substrate; Arlon SQA-TMS-012
508 microns
20.0 mil
Overall thickness; Arlon SQA-TMS-012
Mechanical Properties Metric English Comments
Hardness, Shore A 52
52
Silicone Property; Arlon SQA-TMS-014
Tensile Strength 8.839 MPa
1282 psi
Silicone Property; Arlon SQA-TMS-009
Elongation at Break 29 %
29 %
Tape Property; Arlon SQA-TMS-048
735 %
735 %
Silicone Property; Arlon SQA-TMS-009
Tear Strength 32.8 kN/m
187 pli
Die B; Silicone Property; Arlon SQA-TMS-029
Peel Strength 0.701 kN/m
4.00 pli
Adhesion Strength; Arlon SQA-TMS-047
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 22.0 kV/mm
558 kV/in
Arlon SQA-TMS-020
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature 21.1 °C
12.0 Month

@Temperature 70.0 °F
Descriptive Properties Value Comments
Color Black
Product
Naturally White
Substrate
Tensile Strength (Lb/in) 90
Tape Property; Arlon SQA-TMS-048
Users viewing this material also viewed the following: