Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 20.2 kN/m | 115 pli | ASTM D624 |
Noble Polymers Ecobarrier™ 0712 Thermoplastic Olefin (TPO) Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa.. |
|||
Tear Strength | 20.2 kN/m | 115 pli | ASTM D624 |
Noble Polymers Ecobarrier™ 0916 Thermoplastic Olefin (TPO) Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa.. |
|||
Tear Strength | 20.2 kN/m | 115 pli | Die 'C'; ASTM D624 |
DSM Biomedical PurSil® AL 5 Aliphatic Thermoplastic Silicone Polyether Urethane
(discontinued **) PurSil® AL is a family of aliphatic, thermoplastic silicone polyether urethane copolymers. These polymers are formed by the incorporation of silicone in the polymer backbone together with polyether.. |
|||
Tear Strength | 20.2 - 226 kN/m | 115 - 1290 pli | Average value: 102 kN/m Grade Count:7 |
Overview of materials for Polypropylene, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Tear Strength | 20.2 kN/m | 115 pli | 2 in/min; ASTM D624 |
A. Schulman POLYPUR™ FPU 1109 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tear Strength | 20.2 kN/m | 115 pli | 2 in/min; ASTM D624 |
A. Schulman POLYPUR™ FPU 1109 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tear Strength | 20.2 kN/m | 115 pli | 2 in/min; ASTM D624 |
A. Schulman POLYPUR™ FPU 1109 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tear Strength | 20.2 kN/m | 115 pli | 2 in/min; ASTM D624 |
A. Schulman POLYPUR™ FPU 1109 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tear Strength | 20.2 kN/m | 115 pli | 2 in/min; ASTM D624 |
A. Schulman POLYPUR™ FPU 1109 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tear Strength | 20.2 kN/m | 115 pli | Silicone Property; ASTM D624 |
Arlon 28561R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1528 FiberglassSide 2: Uncured Silicone RubberInterleave 2: PolyethyleneAppearance: Red silicone gum o.. |
|||
Tear Strength | 20.2 kN/m | 115 pli | cured for 72 hrs @ RT |
ACC QM 118 QSI Quantum Silicones 18 Durometer Condensation Cured Moldmaking Material QM 107 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is an.. |
|||
Tear Strength | 20.2 kN/m | 115 pli | cured 72 hrs @ RT |
ACC QM 122 QSI Quantum Silicones 22 Durometer Condensation Cured Moldmaking Material QM 122 is a two-component, room temperature condensation cure silicone material. The cured rubber is flexible with excellent mechanical and physical properties in addition to good shelf-life stabili.. |
|||
Tear Strength | 20.2 kN/m | 115 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® IT 09-021 Natural Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerUV StabilizedOpaqueApplications:General PurposeMarket:Consumer GoodsAutomotiveProcessing Method:Injection MoldingInformation provided by Pol.. |
|||
Tear Strength | 20.2 kN/m | 115 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® IT 38-113 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerNaturalUV StabilizedApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Injection MoldingPolyOne First Cho.. |
|||
Tear Strength | 20.2 kN/m | 115 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® RT-3840MS Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerTransparentUV StabilizedApplications:Multi-PurposeMarket:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceInformation.. |
|||
Tear Strength | 20.2 kN/m | 115 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® RT-3840MS Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerTransparentUV StabilizedApplications:Multi-PurposeMarket:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceInformation.. |
|||
Tear Strength | 20.2 - 175 kN/m | 115 - 999 pli | Average value: 72.6 kN/m Grade Count:19 |
Overview of materials for Silicone Polyurethane, Ether Based This property data is a summary of similar materials in the MatWeb database for the category "Silicone Polyurethane, Ether Based". Each property range of values reported is minimum and maximum value.. |
|||
Tear Strength | 20.2 kN/m | 115 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® RT-3740 Thermoplastic Elastomer - SBC, Mineral Filled
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledNaturalApplications:General PurposeMarket:Consumer GoodsIndustrialBuilding and ConstructionProcessing Method:Injection Molding.. |
|||
Tear Strength | 20.2 kN/m | 115 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® RT-3840M Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerNaturalApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceDisclaimer.. |
|||
Tear Strength | 20.2 kN/m | 115 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® ST-6140 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerNaturalOver-Molding GradeApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Injection MoldingPolyOne Firs.. |
|||
Tear Strength | 20.2 kN/m | 115 pli | 2 in/min; ASTM D624 |
A. Schulman POLYPUR™ FPU 1109 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |