Mechanical Properties Metric English Comments
Tear Strength 20.1 kN/m
115 pli
ISO 34
Multibase TPSiV® 4000-50A Thermoplastic Elastomer
FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; UV stableAPPLICATIONS: Solution for soft touch overmolding on consumer electronics, mob..
Tear Strength 20.2 kN/m
115 pli
ASTM D624
Noble Polymers Ecobarrier™ 0712 Thermoplastic Olefin (TPO)
Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa..
Tear Strength 20.2 kN/m
115 pli
ASTM D624
Noble Polymers Ecobarrier™ 0916 Thermoplastic Olefin (TPO)
Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa..
Tear Strength 20.2 kN/m
115 pli
Die 'C'; ASTM D624
DSM Biomedical PurSil® AL 5 Aliphatic Thermoplastic Silicone Polyether Urethane  (discontinued **)
PurSil® AL is a family of aliphatic, thermoplastic silicone polyether urethane copolymers. These polymers are formed by the incorporation of silicone in the polymer backbone together with polyether..
Tear Strength 20.2 - 226 kN/m
115 - 1290 pli
Average value: 102 kN/m Grade Count:7
Overview of materials for Polypropylene, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri..
Tear Strength 20.1 kN/m
115 pli
Die C, 510 mm/min; ASTM D624
PolyOne Synprene® RT-3750 Styrene Butadiene Block Copolymer (SBC) with Mineral Filler  (discontinued **)
Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom..
Tear Strength 20.2 kN/m
115 pli
2 in/min; ASTM D624
A. Schulman POLYPUR™ FPU 1109 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Tear Strength 20.2 kN/m
115 pli
2 in/min; ASTM D624
A. Schulman POLYPUR™ FPU 1109 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Tear Strength 20.2 kN/m
115 pli
2 in/min; ASTM D624
A. Schulman POLYPUR™ FPU 1109 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Tear Strength 20.2 kN/m
115 pli
2 in/min; ASTM D624
A. Schulman POLYPUR™ FPU 1109 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Tear Strength 20.2 kN/m
115 pli
2 in/min; ASTM D624
A. Schulman POLYPUR™ FPU 1109 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Tear Strength 20.2 kN/m
115 pli
Silicone Property; ASTM D624
Arlon 28561R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1528 FiberglassSide 2: Uncured Silicone RubberInterleave 2: PolyethyleneAppearance: Red silicone gum o..
Tear Strength 20.2 kN/m
115 pli
cured for 72 hrs @ RT
ACC QM 118 QSI Quantum Silicones 18 Durometer Condensation Cured Moldmaking Material
QM 107 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is an..
Tear Strength 20.2 kN/m
115 pli
cured 72 hrs @ RT
ACC QM 122 QSI Quantum Silicones 22 Durometer Condensation Cured Moldmaking Material
QM 122 is a two-component, room temperature condensation cure silicone material. The cured rubber is flexible with excellent mechanical and physical properties in addition to good shelf-life stabili..
Tear Strength 20.2 kN/m
115 pli
Die C (graves), 20 in/min; ASTM D624
PolyOne Synprene® IT 09-021 Natural Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:Multi-Purpose Thermoplastic ElastomerUV StabilizedOpaqueApplications:General PurposeMarket:Consumer GoodsAutomotiveProcessing Method:Injection MoldingInformation provided by Pol..
Tear Strength 20.2 kN/m
115 pli
Die C (graves), 20 in/min; ASTM D624
PolyOne Synprene® IT 38-113 Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerNaturalUV StabilizedApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Injection MoldingPolyOne First Cho..
Tear Strength 20.2 kN/m
115 pli
Die C (graves), 20 in/min; ASTM D624
PolyOne Synprene® RT-3840MS Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerTransparentUV StabilizedApplications:Multi-PurposeMarket:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceInformation..
Tear Strength 20.2 kN/m
115 pli
Die C (graves), 20 in/min; ASTM D624
PolyOne Synprene® RT-3840MS Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerTransparentUV StabilizedApplications:Multi-PurposeMarket:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceInformation..
Tear Strength 20.2 - 175 kN/m
115 - 999 pli
Average value: 72.6 kN/m Grade Count:19
Overview of materials for Silicone Polyurethane, Ether Based
This property data is a summary of similar materials in the MatWeb database for the category "Silicone Polyurethane, Ether Based". Each property range of values reported is minimum and maximum value..
Tear Strength 20.2 kN/m
115 pli
Die C (graves), 20 in/min; ASTM D624
PolyOne Synprene® RT-3740 Thermoplastic Elastomer - SBC, Mineral Filled  (discontinued **)
Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledNaturalApplications:General PurposeMarket:Consumer GoodsIndustrialBuilding and ConstructionProcessing Method:Injection Molding..
Tear Strength 20.2 kN/m
115 pli
Die C (graves), 20 in/min; ASTM D624
PolyOne Synprene® RT-3840M Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerNaturalApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceDisclaimer..
Tear Strength 20.2 kN/m
115 pli
Die C (graves), 20 in/min; ASTM D624
PolyOne Synprene® ST-6140 Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerNaturalOver-Molding GradeApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Injection MoldingPolyOne Firs..
Tear Strength 20.2 kN/m
115 pli
2 in/min; ASTM D624
A. Schulman POLYPUR™ FPU 1109 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.