Polymer Property : Tear Strength = 241 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 241 kN/m
1380 pli
ASTM D1004
Radici Heraflex® E 6521 TPC-ET Thermoplastic Elastomer
TPC-ET Thermoplastic Elastomer. Medium-high Modulus, Nominal Shore D/15s 57. Natural colorProcessing technology: Injection moldingInformation provided by Radici group.