Material Notes:
TPC-ET Thermoplastic Elastomer. Medium-high Modulus, Nominal Shore D/15s 57. Natural colorProcessing technology: Injection moldingInformation provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.23 g/cc
1.23 g/cc
Water Absorption 0.20 %

@Time 86400 sec
0.20 %

@Time 24.0 hour
MI / 08
Melt Flow 23 g/10 min

@Load 2.16 kg,
Temperature 230 °C
23 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
Instantaneous; ISO 868
57

@Time 15.0 sec
57

@Time 0.00417 hour
ISO 868
Tensile Strength at Break 49.0 MPa
7110 psi
ISO 527-1/2
Elongation at Break 634 %
634 %
ISO 527 1/2
Flexural Modulus 0.342 GPa
49.6 ksi
ISO 178/1A
Izod Impact, Notched NB
NB
ASTM D256
Tear Strength 241 kN/m
1380 pli
ASTM D1004
Abrasion 20
20
mm<sup>3</sup>; DIN 53516
Thermal Properties Metric English Comments
Melting Point 210 °C
410 °F
Vicat Softening Point 195 °C

@Load 5.10 kg
383 °F

@Load 11.2 lb
50°C/h
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Electrical Properties Metric English Comments
Comparative Tracking Index 600 V
600 V