Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 42.3 kN/m | 241 pli | ASTM D624 |
Multibase Multi-Flex® TPE D 5010 Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tear Strength | 42.2 kN/m | 241 pli | post cured- 2 hours at 177°C; Die B |
Multibase SILASTIC® C7-4565 CADOX TS-50S Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tear Strength | 42.2 kN/m | 241 pli | B-type, Vulcanized |
KKPC KOSYN 1712G Styrene Butadiene Rubber Styrene Butadiene RubberCharacteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and.. |
|||
Tear Strength | 42.2 kN/m | 241 pli | B-type, Vulcanized |
KKPC KOSYN 1712H Styrene Butadiene Rubber Styrene Butadiene RubberCharacteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and.. |
|||
Tear Strength | 42.2 kN/m | 241 pli | Die B, no post cure; ASTM D624 |
Multibase C6-165 Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tear Strength | 42.2 kN/m | 241 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 50A, Black Peroxide Cure Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 42.2 kN/m | 241 pli | |
Dow Corning S70 LIQUID SILICONE RUBBER KIT A heat-cured elastomer for use by customers fabricating medical devices, including those intended for implantation in humans for less than 30 days and non-implant applications. Dow Corning® S70 Liq.. |
|||
Tear Strength | 42.2 kN/m | 241 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 50A, Black Peroxide Cure Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |