Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 4.38 kN/m | 25.0 pli | ASTM D624 |
Parker Chomerics Tecknit Consil®-C 871 Silver-Copper Filled Silicone Elastomer Description: CONSIL-C is a silicone or fluorosilicone elastomer filled with silver-plated copper particles designed to achieve maximum electrical conductivity. CONSIL-C provides one of the highest s.. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | ASTM D624 |
Parker Chomerics Tecknit Consil®-R 856 Pure Silver-Filled Silicone Elastomer Description: CONSIL-R 856 offers the lowest durometer available for pure silver-filled elastomerTypical Applications: CONSIL-R is designed for use in low to moderate pressure applicationsInformation.. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | Die C; ASTM D624 |
Monmouth Rubber & Plastics Durafoamâ„¢ C44 Closed Cell Epichlorohydrin Information provided by Monmouth Rubber & Plastics Corp. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | Die B |
Lord Adhesives Circalokâ„¢ 6715 Silicone Encapsulant Circalokâ„¢ 6715 is a two component, medium viscosity, solvent-free silicone which cures at room temperature to an elastomeric, stress-free rubber of outstanding electrical and high temperature p.. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | Initial Tear Strength |
Saint-Gobain CHR® 2265-2 Extruded PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu.. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | Initial Tear Strength |
Saint-Gobain CHR® HM426 High Modulus PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu.. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | Initial Tear Strength |
Saint-Gobain CHR® HM430 High Modulus PTFE Film Backing Acrylic Adhesive Pressure Sensitive Tape Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu.. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | Initial Tear Strength |
Saint-Gobain CHR® M60 Polyester Film Backing Acrylic Adhesive Pressure Sensitive Tape Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low water absorptio.. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | Initial Tear Strength |
Saint-Gobain CHR® M66 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | Initial Tear Strength |
Saint-Gobain CHR® M69 Polyester Film Backing Acrylic Adhesive Pressure Sensitive Tape Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low water absorptio.. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | Initial Tear Strength |
Saint-Gobain CHR® M705 Polyester Film Backing Acrylic Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | Initial Tear Strength |
Saint-Gobain CHR® M716 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | Initial Tear Strength |
Saint-Gobain CHR® M717 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | Initial Tear Strength |
Saint-Gobain CHR® M758 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | Initial Tear Strength |
Saint-Gobain CHR® M765 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | Initial Tear Strength |
Saint-Gobain CHR® M797 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | Initial Tear Strength |
Saint-Gobain CHR® M823 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | Initial Tear Strength |
Saint-Gobain CHR® M824 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | Initial Tear Strength |
Saint-Gobain CHR® M851 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | Initial Tear Strength |
Saint-Gobain CHR® M887 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | Initial Tear Strength |
Saint-Gobain CHR® M97 Polyester Film Backing Acrylic Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | Initial Tear Strength |
Saint-Gobain CHR® M50 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | Initial Tear Strength |
Saint-Gobain CHR® M52 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | |
Dow Corning 752 ADHESIVE/SEALANT General purpose silicone adhesive/sealantInformation provided by Dow Corning |
|||
Tear Strength | 4.38 - 7.01 kN/m | 25.0 - 40.0 pli | ASTM D624 |
Parker Chomerics CHO-SEAL 1215 Conductive Elastomer Resists highest level of EMP induced current; military gasket of choice in non-corrosive environments; excellent processing for molding and extrusion. Molded and ExtrudedRoHS Compliant Information p.. |